تنش‌های پسماند در جوش‌های لب به لب اتصالات لوله غیرمشابه

Effect of the welding heat input on residual stresses in butt-welds of dissimilar pipe joints

اثر ورودی حرارت جوشکاری بر تنش‌های پسماند در جوش‌های لب به لب اتصالات لوله غیرمشابه

ABSTRACT

This study used finite element techniques to analyse the thermo-mechanical behaviour and residual stresses in dissimilar butt-welded pipes. The residual stresses at the surface of some weld specimens were measured experimentally by using the hole-drilling method. The results of the finite element analysis were compared with experimentally measured data to evaluate the accuracy of the finite element modelling. Based on this study, a modelling procedure with reasonable accuracy was developed. The developed finite element modelling was used to study the effects of welding heat input on magnitude and distribution of welding residual stresses in butt-welded pipes made of ferritic and austenitic steels. The hoop and axial residual stresses in dissimilar pipe joints of 8 mm thick for V-groove shape were studied. It is shown that the welding heat input has a significant effect on magnitude and distribution of residual stresses in the stainless steel side of the studied joints.

 

  

ادامه مطلب ...

چقرمگی شکست یک فولاد ضدزنگ سوپر داپلکس جوشکاری شده

Fracture toughness of a welded super duplex stainless steel

چقرمگی شکست یک فولاد ضدزنگ سوپر داپلکس جوشکاری شده

ABSTRACT

Fracture toughness testing was conducted on standard single-edge notched bend bar specimens of base and weld metal. The material was the SAF 2906 super duplex stainless steel. The aim was to evaluate the susceptibility for brittle failure at sub-zero temperatures for the base and weld metal. The base metal was tested between −103 and −60 °C and was evaluated according to the crack-tip opening displacement method. The fracture event at and below −80 °C can be described as ductile until critical cleavage initiation occurs, which caused unstable failure of the specimen. The welding method used was submerged arc welding with a 7 wt% nickel filler metal. The welded specimens were post-weld heat treated (PWHT) at 1100 °C for 20 min and then quenched. Energy-dispersive X-ray spectroscopy analysis showed that during PWHT substitutional element partitioning occurred which resulted in decreased nickel content in the ferrite. The PWHT weld metal specimens were tested at −72 °C. The fracture sequence was critical cleavage fracture initiation after minor crack-tip blunting and ductile fracture.

 جهت دانلود رایگان نسخه لاتین این مقاله اینجا کلیک کنید .

 

 